Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 250 cP @Temperature 25.0 °C |
250 cP @Temperature 77.0 °F |
of Solution, 5% wt/wt in Styrene |
Polimeri Europa Intene® 60 AF Butadiene Rubber Intene® 60 AF is a solution polymerized low cis polybutadiene produced using an alkyl lithium catalyst. A TNPP/BHT free, food contact approved, non-staining antioxidant is added during the product.. |
|||
Viscosity | 250 - 350 cP | 250 - 350 cP | |
ND Industries SuperGlue Ethyl 300 General DescriptionA medium to low viscosity cyanoacrylate which is used for bonding plastics and rubber in various combinations.Meets military spec Mil-A-46050C Type II Class II |
|||
Viscosity | 250 cP @Temperature 30.0 °C |
250 cP @Temperature 86.0 °F |
|
Proto3000 Accura® 25 Plastic Stereolithography (SLA) Prototyping Polymer Description: A high stiffness engineered nanocomposite that opens new applications for stereolithography users. Features: Look and feel of molded polypropyleneOutstanding feature resolution and accu.. |
|||
Viscosity | 250 - 350 cP @Temperature 82.2 °C |
250 - 350 cP @Temperature 180 °F |
|
Northstar Polymers SBA-036 Polyester Curing Agent Information provided by Northstar Polymers. |
|||
Viscosity | 250 - 600 cP | 250 - 600 cP | |
Huntsman AroCy B-30 Prepolymer Bisphenol-A Dicyanate Comments/Applications: Max color is 8. Prepolymer of B-10. Used primarily in the manufacture of prepreg for structural composites and tooling. High temperature adhesives.Data provided by Ciba Spe.. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | 10% Toluene Solution at 25°C; KM 06 |
Kraton® G1654 E (SEBS) Linear Triblock Copolymer Description: Kraton G1654 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass. It is supplied from Europe in the physical .. |
|||
Viscosity | 250 cP @Temperature 25.0 °C |
250 cP @Temperature 77.0 °F |
|
Silikony Polskie Polsil OM 250 Methyl Silicone Fluid The methyl silicone fluids are liquid organic silicone polymers, including inorganic elements (Si-O bond, as in quartz, glass or sand) and inorganic elements (methyl groups) in one molecule. This gi.. |
|||
Viscosity | 250 - 1000 cP | 250 - 1000 cP | |
Solvay ALKAMULS® EL 620 Surfactant Description: Castor oil ethoxylate (30 EO) Emulsifier for fats, oils fatty acids and solvents. Maintains stability of oil-in-water emulsions over a wide temperature range as co-emulsifier with an HL.. |
|||
Viscosity | <= 250 cP | <= 250 cP | |
Solvay RHODASURF® L-7/90 Surfactant Chemical Name: NONIONIC EMULSIFIERAvailable in: Asia Pacific, Europe, Latin America and North America Applications: RHODASURF© L 7 90 is an excellent primary nonionic surfactant recommended espec.. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | Part B |
Master Bond EP30HV Optically Clear, High Strength Two Part Epoxy Description: Master Bond EP30HV is a lower viscosity, two component epoxy system for high performance bonding, sealing, coating and potting. It is formulated to cure at room temperature or more rapi.. |
|||
Viscosity | 250 - 400 cP | 250 - 400 cP | Part B |
Master Bond EP41S-1HT Solvent Resistant Adhesive, Sealant and Coating Description: Master Bond EP41S-1HT is a two component epoxy resin system for high performance bonding, sealing, coating and encapsulating. It has a 100 to 30 mix ratio by weight and is formulated to.. |
|||
Viscosity | 250 cP | 250 cP | |
Von Roll Isola IMI Varnish 73538 Solventless Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: 30°C. Usag.. |
|||
Viscosity | 250 cP | 250 cP | |
Von Roll Isola IMI Varnish 9637 Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 29°C. Average solids: 48%. Usage Notes: Treating transformers, magnet coils, stators, fields, armatures, railway field coils, and bare copper coils... |
|||
Viscosity | 250 - 950 cP @Temperature 190 °C |
250 - 950 cP @Temperature 374 °F |
542-111 |
Westlake Epolene® N-15 Nonemulsifiable - Low Molecular Weight Polypropylene Polymer Product Description: Epolene N-15 is a low viscosity polypropylene homopolymer with a high melt point and excellent hardness. Epolene N-15 is used in color concentrates, toner compounds, and as a pi.. |
|||
Viscosity | 250 - 950 cP | 250 - 950 cP | 542-111 |
Westlake Epolene® N-15P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-15P is a low viscosity polypropylene homopolymer powder with a high melt point and excellent hardness. Epolene N-15P is used in color concentrates, toner compounds, and as a p.. |
|||
Viscosity | 250 - 450 cP | 250 - 450 cP | 542-111 |
Westlake Epolene® N-21P Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Description: Epolene N-21P is a medium density polyethylene that improves slump resistance in cable filling and flooding, provides lubricity in printing inks, and can be used as a viscosity modifier.. |
|||
Viscosity | 250 cP @Temperature 25.0 °C |
250 cP @Temperature 77.0 °F |
After mixing |
Tra-Con Tra-Bond 2115 Clear High Strength Epoxy Adhesive TRA-BOND 2115 is a clear, low viscosity epoxy formulation used in the fabrication of lasers. It is capable of withstanding 30 seconds of 60 watt direct laser energy. The low cure shrinkage (using a .. |
|||
Viscosity | 250 - 350 cP | 250 - 350 cP | |
Dow CYRACURE™ UVR-6107 Cycloaliphatic Epoxide CYRACURE™ UVR-6107 cycloaliphatic epoxide is a low viscosity base resin. Typical applications include: Metal decoration coatings Overprint varnishes Information provided by Dow |
|||
Viscosity | 250 cP | 250 cP | Dynamic |
Dow Corning SYL-OFF® PMCPSL 700 Coating Information provided by Dow Corning |
|||
Viscosity | 250 - 300 cP @Temperature 30.0 °C |
250 - 300 cP @Temperature 86.0 °F |
|
3D Systems Accura® Xtreme Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systemsApplicationsForm, fit and function prototypesDurable AssembliesSnap fit assembliesTough enclosuresConsumer electronic componentsMaster patte.. |
|||
Viscosity | 250 - 750 cP | 250 - 750 cP | |
3M Fastbond™ 2000-NF Contact Adhesive with Spray Activator #1 3M Fastbond™ Contact Adhesive 2000-NF with Spray Activator #1 is a water-dispersed, high solid, activated adhesive which provides immediate bonding capabilities and handling strength without forced.. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco HiE-Coat™ 840-MS High Emissivity Silicone-Ceramic Coating 840-C is a silicone-ceramic, black-pigmented coating for aluminum, brass, copper, and carbon and stainless steels to 1100 ºF (593 ºC).The HiE-Coat™ line of high emissivity coatings are black-body.. |
|||
Viscosity | 250 - 350 cP | 250 - 350 cP | |
Aremco Corr-Paint™ CP4050-S High Temperature Protective Coating Silicone-Polyester |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco Lamp-Coat™ LC4040-SG High Temperature Coating, Silicone White reflective coating for use on mercury vapor lamps and other high temperature glass and quartz components to 1200 ºF (649 ºC). |
|||
Viscosity | 250 cP @Temperature 30.0 °C |
250 cP @Temperature 86.0 °F |
|
3D Systems Accura® 25 Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systems.ApplicationsFunctional components for assemblies and mock-ups for:Automotive styling parts — trim, fascia, and other componentsConsumer el.. |
|||
Viscosity | 250 - 450 cP @Temperature 125 °C |
250 - 450 cP @Temperature 257 °F |
542-111 |
Westlake Epolene® N-11 Nonemulsifiable - Low Molecular Weight Polyethylene Polymer Product Description: Epolene N-11 is a polyethylene (PE) homopolymer that can easily be melt blended with natural or synthetic waxes to increase the tensile strength of wax blends, improve the gloss.. |
|||
Viscosity | 250 cP | 250 cP | Part B |
Resinlab® UR1049 MDI Based Rigid Polyurethane Foam System Resinlab™ UR 1049 is a, two component, water blown, 4 lb per cubic foot, MDI based rigid polyurethane foam system. It is designed to cure completely at room temperature. Being of a closed cell stru.. |