Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 122 kV/mm | 3100 kV/in | |
Von Roll Isola IMI Varnish 74035 Solventless Epoxy Varnish for Electrical Insulation Data provided by Von Roll Isola USA.IMI solventless resins provide relatively void-free insulation for greater protection against severe environments and corona breakdown. Flash Point: >99°C. Usa.. |
|||
Dielectric Strength | 122 kV/mm | 3100 kV/in | |
Von Roll Isola IMI Varnish 9637 Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 29°C. Average solids: 48%. Usage Notes: Treating transformers, magnet coils, stators, fields, armatures, railway field coils, and bare copper coils... |
|||
Dielectric Strength | 122 kV/mm | 3100 kV/in | |
Von Roll Isola IMI Varnish 9637AP Polyester Varnish for Electrical Insulation Data provided by Von Roll Isola USA.Flash Point: 53°C. Average solids: 48%. Usage Notes: Higher flash point version of IMI 9637 |