Voloknohim PA-SV30 Glass and Mineral Filled

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Voloknohim
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Voloknohim PA-SV30 Glass and Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Voloknokhim
Physical Properties Metric English Comments
Filler Content 27 - 33 %
27 - 33 %
Particle Size 2000 - 5000 µm
2000 - 5000 µm
at least 97%
Linear Mold Shrinkage 0.0040 - 0.0080 cm/cm
0.0040 - 0.0080 in/in
Mechanical Properties Metric English Comments
Elongation at Break >= 3.0 %
>= 3.0 %
Modulus of Elasticity 7.20 GPa
1040 ksi
When curved
Transverse Strength >= 200 MPa
>= 29000 psi
when destroyed
Tear Strength Test >= 155
>= 155
MPa
Users viewing this material also viewed the following: