UBE UBEPOL BR34HL HIPS (stirring rate = 400 rpm)

Category Polymer , Thermoplastic , Polystyrene (PS) , Polystyrene, Impact Modified
Manufacturer UBE
Trade Name UBEPOL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF UBE UBEPOL BR34HL HIPS (stirring rate = 400 rpm).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: UBEPOL-BR34HL is characterized by its lower molecular weight and higher linear molecular chain compared with UBEPOL-BR15HB. The properties of HIPS modified by UBEPOL-BR34HL are very good, and especially much better than the other grades in respect of ballance between gloss and impact resistance. Information provided by UBE.
Physical Properties Metric English Comments
Particle Size 1.23 µm
1.23 µm
Rubber Particle Size
Melt Flow 2.7 g/10 min
2.7 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength at Break 30.0 MPa
4350 psi
Tensile Strength, Yield 31.0 MPa
4500 psi
Elongation at Break 43 %
43 %
Izod Impact, Notched 0.790 J/cm
1.48 ft-lb/in
Thermal Properties Metric English Comments
Vicat Softening Point 101 °C
214 °F
Optical Properties Metric English Comments
Gloss 80 %
80 %
Descriptive Properties Value Comments
MEK/Acetone Insolubles (wt.%) 25.2
Swelling Index 11.9