Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.790 J/cm | 1.48 ft-lb/in | ASTM D256 |
Flint Hills P9R6K-054 Random Copolymer Polypropylene Excellent clarity. High flow material. Product does not contain any animal derived components. Phthalate-free.Applications: Injection molding - High clarity applications. A replacement for PET, .. |
|||
Izod Impact, Notched | 0.790 J/cm | 1.48 ft-lb/in | ASTM D256 |
Flint Hills P9R6K-054A Random Copolymer Polypropylene Features: Excellent clarity. High flow material. Product does not contain animal derived components. Phthalate-free.Applications: Injection molding - High clarity applications. A replacement fo.. |
|||
Izod Impact, Notched | 0.790 J/cm | 1.48 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP LUBRICOMP RFL159 PA 66 LNP* LUBRICOMP* RFL159 is a compound based on Nylon 66 resin containing 25% Glass Fiber, 5% PTFE. Added features of this material include: Wear Resistant, Flame Retardant |
|||
Izod Impact, Notched | 0.790 J/cm @Temperature -30.0 °C |
1.48 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Izod Impact, Notched | 0.790 J/cm @Temperature -30.0 °C |
1.48 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Asia Pacific) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Izod Impact, Notched | 0.790 J/cm @Temperature -30.0 °C |
1.48 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL EXNL0353 PPE+HIPS EXNL0353 resin is a modified PPE + PS blend with an excellent balance of non-halogenated flame retardance, hydrolytic stability, impact and heat resistance, good flow, and low specific gravity for l.. |
|||
Izod Impact, Notched | 0.790 J/cm @Temperature -30.0 °C |
1.48 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
SABIC Innovative Plastics NORYL GFN1630V PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1630V Polyphenylene Oxide (PPO) + Polystyrene (PS) resin is a 30 % Glass Reinforced, injection moldable grade with improved hydrolytic stability; this grade has been developed for fluid en.. |
|||
Izod Impact, Notched | 0.790 J/cm | 1.48 ft-lb/in | |
UBE UBEPOL BR34HL HIPS (stirring rate = 400 rpm) Description: UBEPOL-BR34HL is characterized by its lower molecular weight and higher linear molecular chain compared with UBEPOL-BR15HB. The properties of HIPS modified by UBEPOL-BR34HL are very goo.. |
|||
Izod Impact, Notched | 0.790 J/cm @Temperature 23.0 °C |
1.48 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics LNP Thermocomp MF0069S PP LNP* Thermocomp* MF0069S is a compound based on Polypropylene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Chemically Coupled, Flame Retardant, Heat Stabi.. |
|||
Izod Impact, Notched | 0.790 J/cm | 1.48 ft-lb/in | ASTM D256 |
Kolon Kopa® KN173MT40 Nylon 6 Resin KOPA is widely used in the automobile and industrial parts.General KOPA N-6 Features: Good mechanical properties, Extreme toughness, Outstanding self-lubrication and abrasion resistance, Excellent c.. |