Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Trelleborg I644 Antiabrasive SBR Rubber

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Trelleborg
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Trelleborg I644 Antiabrasive SBR Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Styrene-butadiene Rubber is a co-polymer of styrene and butadiene.PropertiesIts general properties are similar to those of natural rubber, but it is more resistant to aging and temperature, and like natural rubber, these properties can be improved further by careful compounding.Due to its unsaturated molecular structure SBR materials tend to have only moderate resistance to tearing, ozone and general weathering. They do not have the same resilience as natural rubber.Resistance to chemicals; good resistance to many inorganic chemical products. Limited resistance to mineral oils, but is not recommended for use with oxidizing acids and general organic liquids.All information provided by Trelleborg
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength, Yield 15.0 MPa
2180 psi
Elongation at Break 400 %
400 %
Tear Strength 45.0 kN/m
257 pli
Abrasion 120
120
mm<sup>3</sup>; 10 N Load
Compression Set 35 %

@Temperature 70.0 °C,
Time 79200 sec
35 %

@Temperature 158 °F,
Time 22.0 hour
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 110 °C
230 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Copyright © lookpolymers.com All Rights Reserved