Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Tipco Tipcolite® VASW 200 Phenolic Compound, Long Glass Fiber, in fluffy form, Medium -Soft Flow & Very High Strength

Category Polymer , Thermoset , Phenolic
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolite® VASW 200 Phenolic Compound, Long Glass Fiber, in fluffy form, Medium -Soft Flow & Very High Strength.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.79 g/cc
0.0647 lb/in³
ASTM D792
Apparent Bulk Density 0.200 g/cc
0.00723 lb/in³
TRM-37
Linear Mold Shrinkage 0.0015 cm/cm
0.0015 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 115 MPa
16700 psi
ASTM D638
Flexural Yield Strength 185 MPa
26800 psi
ASTM D790
Izod Impact, Unnotched (ISO) 45.0 kJ/m²
21.4 ft-lb/in²
ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 3.16e+12 ohm-cm
3.16e+12 ohm-cm
ASTM D257
Surface Resistance 3.16e+12 ohm
3.16e+12 ohm
ASTM D257
Dielectric Strength 15.0 kV/mm
381 kV/in
ASTM D149