Techmer ES HiFill® PSU GF20 BK 20% Glass Filled

Category Polymer , Thermoplastic , Polysulfone (PSU) , Polysulfone, 20% Glass Fiber Reinforced
Manufacturer Techmer ES
Trade Name HiFill®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PSU GF20 BK 20% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
ASTM D792
Water Absorption 0.24 %

@Time 86400 sec
0.24 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cm

@Thickness 3.17 mm
0.0020 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 123
123
ASTM D785
Tensile Strength, Yield 112 MPa
16200 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Flexural Yield Strength 153 MPa
22200 psi
ASTM D790
Flexural Modulus 5.86 GPa
850 ksi
ASTM D790
Izod Impact, Notched 0.801 J/cm

@Thickness 3.17 mm
1.50 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 30.6 µm/m-°C
17.0 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 182 °C
360 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Strength 16.9 kV/mm
430 kV/in
Method A (Short-Time); ASTM D149