Material Notes:
This Material Specification applies to 3 to 100 mm thick plates of the wear-resistant special structural steel XAR® 400.Application: The steel may be used for wear exposed structures, e.g. excavating, mining and earth-moving machinery, truck dump bodies, conveying, crushing and pulverizing equipment, scrap presses, paving moulds and in switch manufacturing.Information Provided by Thyssen Krupp
Mechanical Properties Metric English Comments
Tensile Strength at Break 1250 MPa
181000 psi
Tensile Strength, Yield 1050 MPa
152000 psi
Elongation at Break 12 %
12 %
Charpy Impact 30.0 J

@Temperature -40.0 °C
22.1 ft-lb

@Temperature -40.0 °F
Component Elements Properties Metric English Comments
Aluminum, Al <= 1.0 %
<= 1.0 %
Boron, B <= 0.0050 %
<= 0.0050 %
Carbon, C <= 0.20 %
<= 0.20 %
Chromium, Cr <= 1.0 %
<= 1.0 %
Manganese, Mn <= 1.5 %
<= 1.5 %
Molybdenum, Mo <= 0.50 %
<= 0.50 %
Other <= 0.48 %
<= 0.48 %
Carbon Equivalent
Phosphorous, P <= 0.025 %
<= 0.025 %
Silicon, Si <= 0.80 %
<= 0.80 %
Sulfur, S <= 0.010 %
<= 0.010 %