Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 1250 - 1450 MPa | 181000 - 210000 psi | |
ThyssenKrupp SECURE 450 Structural Steel This Material Specification applies to the liquid-quenched and tempered high-strength special steel SECURE 450 with a hardness between 400 - 480 HBW for civil use from 4 up to 20 mm thickness.Applic.. |
|||
Tensile Strength at Break | 1250 MPa | 181000 psi | |
ThyssenKrupp XAR® 400 Structural Steel This Material Specification applies to 3 to 100 mm thick plates of the wear-resistant special structural steel XAR® 400.Application: The steel may be used for wear exposed structures, e.g. excavati.. |