Mechanical Properties Metric English Comments
Tensile Strength, Yield 1050 MPa

@Strain 0.200 %
152000 psi

@Strain 0.200 %
Haynes 25 alloy, cold worked sheet, 20% cold reduction, aged at 370°C (700°F) for 1 hour
Excellent high-temperature strength with good resistance to oxidizing environments up to 980°C for prolonged exposures and excellent resistance to sulfidation and excellent resistance to metal ga..
Tensile Strength, Yield 1050 MPa
152000 psi
ThyssenKrupp XAR® 400 Structural Steel
This Material Specification applies to 3 to 100 mm thick plates of the wear-resistant special structural steel XAR® 400.Application: The steel may be used for wear exposed structures, e.g. excavati..
Tensile Strength, Yield 1050 MPa

@Strain 0.200 %
152000 psi

@Strain 0.200 %
Typical
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 538°C
High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess..
Tensile Strength, Yield 1050 MPa
152000 psi
R<sub>e</sub>. 500°C tempering temperature. Quenching in oil ø 50. Testpiece hardened by oil quenching from 850°C.
Assab Steels 709M Machinery Steel
ASSAB 709M is an alloyed machinery steel with high strength in small and medium sizes. As standard ASSAB 705M is supplied tough hardened requiring no further heat treatment. It can be oil hardened t..
Tensile Strength, Yield 1050 MPa
152000 psi
Trans.
ATI Wah Chang 425™ Titanium Alloy, Cold Rolled Sheet
ATI 425™ titanium is an innovative high strength alloy that has strength comparable to Ti-6-4, yet has the advantage that it can be cold worked. Originally developed for armor plate for ballistic p..
Tensile Strength, Yield 1048 MPa

@Strain 0.200 %
152000 psi

@Strain 0.200 %
Carpenter Custom 450® Stainless Steel, Condition H1050 (Age Hardened 566°C)
Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T..