MetalTek MTEK WC 9 Cast UNS J42045 Alloy Steel

Category Metal , Ferrous Metal , Alloy Steel
Manufacturer MetalTek
Trade Name MTEK
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek MTEK WC 9 Cast UNS J42045 Alloy Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 229
229
Tensile Strength, Ultimate 480 - 655 MPa
69600 - 95000 psi
Tensile Strength, Yield >= 276 MPa
>= 40000 psi
Elongation at Break >= 20 %
>= 20 %
Component Elements Properties Metric English Comments
Carbon, C 0.05 - 0.18 %
0.05 - 0.18 %
Chromium, Cr 2.0 - 2.75 %
2.0 - 2.75 %
Iron, Fe 94.6 - 96.65 %
94.6 - 96.65 %
As Balance
Manganese, Mn 0.40 - 0.70 %
0.40 - 0.70 %
Molybdenum, Mo 0.90 - 1.2 %
0.90 - 1.2 %
Silicon, Si <= 0.60 %
<= 0.60 %
Descriptive Properties Value Comments
Heat Treatment Quench & Temper