Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ThyssenKrupp PAS 700 Structural Steel for Cold Forming

Category Metal , Ferrous Metal , Carbon Steel , Low Carbon Steel
Manufacturer ThyssenKrupp
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ThyssenKrupp PAS 700 Structural Steel for Cold Forming.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery condition. They offer improved formability and show favorable properties such as low tendency towards hardening and high cold cracking resistance at welding.The steels are used for cold formed parts of different kinds such as truck frames, axle designs and other special profiles and shapes. The entire processing technique is of fundamental importance for the good performance of the products made of these steels. The processor must assure himself, that his calculation, designing and working conform with the material to be used and are suited to the proposed application.If continuous yielding occurs, the yield strength is determined as Rp0,2Information Provided by Thyssen Krupp
Mechanical Properties Metric English Comments
Tensile Strength at Break 750 - 950 MPa
109000 - 138000 psi
Tensile Strength, Yield >= 700 MPa
>= 102000 psi
>= 680 MPa

@Thickness >=8.00 mm
>= 98600 psi

@Thickness >=0.315 in
Elongation at Break >= 12 %
>= 12 %
Charpy Impact 40.0 J

@Temperature -20.0 °C
29.5 ft-lb

@Temperature -4.00 °F
EN 10045
Bend Radius, Minimum 2.0 t
2.0 t
ISO 7438
Component Elements Properties Metric English Comments
Carbon, C <= 0.12 %
<= 0.12 %
Manganese, Mn <= 2.1 %
<= 2.1 %
Niobium, Nb (Columbium, Cb) <= 0.080 %
<= 0.080 %
Phosphorous, P <= 0.025 %
<= 0.025 %
Silicon, Si <= 0.60 %
<= 0.60 %
Sulfur, S <= 0.010 %
<= 0.010 %
Titanium, Ti <= 0.14 %
<= 0.14 %
Users viewing this material also viewed the following: