Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 800 - 950 MPa | 116000 - 138000 psi | |
Schmolz + Bickenbach UGICHROM 4021 Martensitic Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef.. |
|||
Tensile Strength at Break | 750 - 950 MPa | 109000 - 138000 psi | |
ThyssenKrupp PAS 700 Structural Steel for Cold Forming This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio.. |
|||
Tensile Strength at Break | 750 - 950 MPa | 109000 - 138000 psi | |
Schmolz + Bickenbach UGICHROM 244 Chrome Plated Bar Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coeffici.. |