Polymer Property : Tensile Strength, Yield = 700 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 700 MPa
102000 psi
Plansee DENSIMET® D2M Tungsten-Nickel-Molybdenum-Iron Alloy
Characteristics:Easy processingHigh densityPrecision forming and machiningHigh ductilityHigh strength100 % impermeableTypical Applications:Balancing weights in motors and drive componentsVibration d..
Tensile Strength, Yield 700 MPa

@Strain 0.200 %,
Temperature 550 °C
102000 psi

@Strain 0.200 %,
Temperature 1020 °F
Precipitation Hardened prior to test
Special Metals INCOLOY® Alloy 925
A precipitation-hardenable nickel-iron-chromium alloy with additions of molybdenum and copper. It combines the high strength of a precipitation-hardenable alloy with the excellent corrosion resista..
Tensile Strength, Yield 700 MPa

@Strain 0.200 %
102000 psi

@Strain 0.200 %
Precipitation Hardened. Value at room temperature
Special Metals NIMONIC® Alloy PE11
A nickel-iron-chromium alloy precipitation hardened by titanium and aluminum and solid-solution strengthened by an addition of molybdenum. It was developed as a high-strength sheet alloy for use at..
Tensile Strength, Yield 700 - 950 MPa

@Strain 0.200 %
102000 - 138000 psi

@Strain 0.200 %
SSAB Tunnplat Docol® 1000 DP High-strength Steel
High-strength SteelCharacteristics: The steels are annealed at temperatures between 750°C and 850°C, depending on the grade of steel, and then are hardened by quenching in water. Tempering is..
Tensile Strength, Yield >= 700 MPa
>= 102000 psi
SSAB Tunnplat Domex® 700MC HSLA Steel
HSLA SteelCharacteristics: Domex® MC grade steels conform to the provisions of EN 10149-2 standard and often have better properties.Property data is for hot-rolled steel..Domex® is the brand n..
Tensile Strength, Yield 700 MPa
102000 psi
ISO 527
Styrolution Absolan® 2150 SAN
Absolac 2150 Crystal is a heat and chemical resistant gradeInformation provided by Styrolution
Tensile Strength, Yield 700 MPa
102000 psi
ISO 527
Styrolution Absolan® 2300 SAN
Absolac 2300 is a good flow gradeInformation provided by Styrolution
Tensile Strength, Yield >= 700 MPa

@Strain 0.200 %
>= 102000 psi

@Strain 0.200 %
Schmolz + Bickenbach UGICHROM 4057 Martensitic Chrome Plated Bar
Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef..
Tensile Strength, Yield >= 700 MPa

@Strain 0.200 %
>= 102000 psi

@Strain 0.200 %
Schmolz + Bickenbach UGICHROM 4418 Martensitic Chrome Plated Bar
Description: Ugichrom combines the high efficiency of micro-fissuring chromium plating with the technology of Ugitech’s most advanced gradesAdvantages: Zero defects guarantee; Low friction coef..
Tensile Strength, Yield >= 700 MPa
>= 102000 psi
ThyssenKrupp PAS 700 Structural Steel for Cold Forming
This Material Specification applies to plates made of low carbon high strength steels with minimum yield strength values between 315 and 700 MPa1) in the thermo mechanically rolled delivery conditio..
Tensile Strength, Yield 700 MPa

@Temperature 100 °C
102000 psi

@Temperature 212 °F
Wet; EN2561
Hexcel® HexPly® M12 135°C Curing Epoxy Matrix, 45% 46280 Fiber
Information provided by HexCel
Tensile Strength, Yield >= 700 MPa

@Strain 0.200 %
>= 102000 psi

@Strain 0.200 %
CLAL-MSX NICLAFOR® 1000 TD4 Quenched/Cold Rolled, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Tensile Strength, Yield >= 700 MPa

@Strain 0.200 %
>= 102000 psi

@Strain 0.200 %
CLAL-MSX NICLAFOR® 1000 TH1 Quenched/Precipitation Heat Treated, Drawn Copper Alloy
Finished parts can be produced with: reduction in sections, high mechanical properties even at high temperature, high spring properties, high conductivity, good resistance to corrosion, low permeabi..
Tensile Strength, Yield >= 700 MPa

@Strain 0.200 %
>= 102000 psi

@Strain 0.200 %
CLAL-MSX ARCAP Anticorrosion AP1C H14 4/4 hard, Rolled Copper Alloy
Description: The AP1C grade (used in rods for parts that are to be deformed by torsion, bending, riveting, swaging... and for welding) and the AP1 grade (sheet, strip, wire, tubes) is machineable un..
Tensile Strength, Yield 700 MPa
102000 psi
R<sub>e</sub>. 700°C tempering temperature. Quenching in oil ø 50. Testpiece hardened by oil quenching from 850°C.
Assab Steels 709M Machinery Steel
ASSAB 709M is an alloyed machinery steel with high strength in small and medium sizes. As standard ASSAB 705M is supplied tough hardened requiring no further heat treatment. It can be oil hardened t..
Tensile Strength, Yield 700 MPa
102000 psi
min. Re.
Assab Steels 705M Machinery Steel
ASSAB 705M is an alloyed machinery steel with good hardenability also in heavier sizes. As standard ASSAB 705M is supplied tough hardened with no further heat treatment required. It can be oil harde..
Tensile Strength, Yield 700 MPa

@Strain 0.200 %
102000 psi

@Strain 0.200 %
ATI Allegheny Ludlum Stainless Steel AL-6XN® Alloy (UNS N08367), 10% Cold Work
The AL-6XN® alloy is a superaustenitic stainless steel which was developed by Allegheny Ludlum Corporation. It exhibits far greater resistance to chloride pitting, crevice corrosion and stress-co..
Tensile Strength, Yield 700 - 850 MPa
102000 - 123000 psi
ArcelorMittal Complex Phase Steel 1000 Very high strength steel, Cold Rolled Steel
Available in the following: uncoated (HCT980C) and electrogalvanized (HCT980C+ZE)Description: The Complex Phase family of steels supplements ArcelorMittal's VHSS (very high strength steel) product r..
Tensile Strength, Yield 700 - 850 MPa
102000 - 123000 psi
ArcelorMittal Dual Phase 980 LCE Y700 Very high strength steel, Cold Rolled Steel
Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft ..
Tensile Strength, Yield 700 - 850 MPa
102000 - 123000 psi
ArcelorMittal Dual Phase 980 Y700 Very high strength steel, Cold Rolled Steel
Description: Dual Phase steels offer an outstanding combination of strength and drawability as a result of their microstructure, in which a hard martensitic or bainitic phase is dispersed in a soft ..