Teknor Apex Vidux® CV-98-PO323-G79 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade
Manufacturer Teknor Apex Company
Trade Name Vidux®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Vidux® CV-98-PO323-G79 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 105°C Insulation Features: Conductive; Good Abrasion Resistance; Flame Retardant; Good Wear Resistance Uses: Tubing Forms: BlackInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
15 seconds; ASTM D2240
85
85
ASTM D2240
Tensile Strength at Break 6.89 MPa
1000 psi
ASTM D638
Elongation at Break 300 %
300 %
ASTM D638
Taber Abrasion, mg/1000 Cycles 0.41
0.41
2000 Cycles, 1000 g, H-22 Wheel; ASTM D1044
Electrical Properties Metric English Comments
Volume Resistivity 140 ohm-cm
140 ohm-cm
ASTM D257
Surface Resistance 120 ohm
120 ohm
ASTM D257
Descriptive Properties Value Comments
Appearance Black