Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 120 ohm | 120 ohm | ASTM D257 |
Teknor Apex Vidux® CV-98-PO323-G79 Polyvinyl Chloride, Flexible Notes: 105°C Insulation Features: Conductive; Good Abrasion Resistance; Flame Retardant; Good Wear Resistance Uses: Tubing Forms: BlackInformation Provided by Teknor Apex |
|||
Surface Resistance | 120 ohm | 120 ohm | |
LATI Latiohm 75/4-03 PD01 G/20 PBT, 20% Glass Fiber Reinforced Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Surface Resistance | 120 ohm | 120 ohm | |
LATI Latiohm 75/4-08 PD01 G/30 PBT, 30% Glass Fiber Reinforced Semiconductive/dissipative product based on Polybutylene Terephthalate (PBT). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |