Teknor Apex UNIPRENE® 7100-87 Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Teknor Apex Company
Trade Name UNIPRENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex UNIPRENE® 7100-87 Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Teknor Apex Company
Physical Properties Metric English Comments
Specific Gravity 0.930 g/cc
0.930 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 89
89
5 seconds; ASTM D2240
93
93
Instantaneous; ASTM D2240
Tensile Strength, Yield 11.4 MPa
1650 psi
ASTM D412
Elongation at Break 400 %
400 %
ASTM D412
100% Modulus 0.00655 GPa
0.950 ksi
ASTM D412
Tear Strength 56.1 kN/m
320 pli
ASTM D624
Compression Set 38 %
38 %
23°C, 22 hr.; ASTM D395, Method B
59 %
59 %
100°C, 22 hr.; ASTM D395, Method B
Thermal Properties Metric English Comments
Brittleness Temperature <= -60.0 °C
<= -76.0 °F
ASTM D746