Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

CENTROPLAST CENTROLEN PP TV Polypropylene + talc

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer CENTROPLAST Engineering Plastics GMBH
Trade Name CENTROLEN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF CENTROPLAST CENTROLEN PP TV Polypropylene + talc.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This material is a low density, easily machined plastic that has good damping properties and is reinforced with talc for high rigidity. Applications include components for the electrical industry, housings and covers.Information provided by CENTROPLAST Engineering Plastics GMBH
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Ball Indentation Hardness 90.0 MPa
13100 psi
value at 30 sec.; ISO 2039-1
Tensile Strength, Yield 33.0 MPa
4790 psi
v = 50 mm/min; ISO 527-2
Elongation at Break >= 6.0 %
>= 6.0 %
ISO 527-2
Tensile Modulus 3.80 GPa
551 ksi
ISO 527-2
Charpy Impact Unnotched 3.00 J/cm²
14.3 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.300 J/cm²
1.43 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 100 °C
212 °F
Long Term
130 °C
266 °F
Short term
Deflection Temperature at 1.8 MPa (264 psi) >= 75.0 °C
>= 167 °F
ISO 75-2
Users viewing this material also viewed the following: