Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Teknor Apex Sinvicomp SIH 5005A Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name Sinvicomp
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex Sinvicomp SIH 5005A Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: Asia Pacific Features: Good Stiffness Uses: Wire and Cable Applications Wire Types: V-90HT Agency Ratings: AS 3147-1992 Forms: Pellets Processing Method: ExtrusionInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.41 g/cc
1.41 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 91
91
ASTM D2240
Tensile Strength, Yield 17.00 MPa
2465 psi
Change in tensile strength after 504 hours at 248°F; ASTM D638
20.0 MPa
2900 psi
9.8 in/min; ASTM D638
Elongation at Break 208 %
208 %
Change after 504 hours at 248°F; ASTM D638
260 %
260 %
9.8 in/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 190 °C

@Time >=7200 sec
374 °F

@Time >=2.00 hour
Congo Red; BS 2782
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm

@Temperature 20.0 °C
1.00e+14 ohm-cm

@Temperature 68.0 °F
BS 2782