Material Notes:
Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact AcceptableUses: Shrink Wrap Forms: Pellets Processing Method: Blown FilmInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Melt Flow 54.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
54.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 76
76
ASTM D2240
Tensile Strength, Yield 44.6 MPa
6470 psi
9.8 in/min; ASTM D638
Elongation at Break 160 %
160 %
9.8 in/min; ASTM D638
Izod Impact, Notched 0.801 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 77.8 °C
172 °F
ASTM D1525