| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Specific Gravity | 0.890 g/cc | 0.890 g/cc | ASTM D792 |
| Melt Flow | 4.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 75 | 75 | ASTM D2240 |
| Tensile Strength at Break | 12.4 MPa | 1800 psi | ASTM D412 |
| Elongation at Break | 650 % | 650 % | ASTM D412 |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Rear Barrel Temperature | 182 - 232 °C | 360 - 450 °F | |
| Middle Barrel Temperature | 188 - 238 °C | 370 - 460 °F | |
| Front Barrel Temperature | 193 - 243 °C | 380 - 470 °F | |
| Nozzle Temperature | 199 - 249 °C | 390 - 480 °F | |
| Zone 1 | 182 - 232 °C | 360 - 450 °F | |
| Zone 2 | 188 - 238 °C | 370 - 460 °F | |
| Zone 3 | 193 - 243 °C | 380 - 470 °F | |
| Zone 5 | 199 - 249 °C | 390 - 480 °F | |
| Die Temperature | 199 - 249 °C | 390 - 480 °F | |
| Melt Temperature | 199 - 249 °C | 390 - 480 °F | Processing Temperature |
| Mold Temperature | 35.0 - 48.9 °C | 95.0 - 120 °F | |
| Injection Pressure | 1.38 - 5.52 MPa | 200 - 800 psi | |
| Back Pressure | 0.172 - 0.689 MPa | 25.0 - 100 psi | |
| Cushion | 0.381 - 2.54 cm | 0.150 - 1.00 in | |
| Screw Speed | 50 - 100 rpm | 50 - 100 rpm |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Appearance | Opaque |