Material Notes:
Notes: 105°C Insulation; RoHS Compliant Features: Flame Retardant; High Heat Resistance; Low Temperature Flexibility Uses Wet Rated Insulation Wire Types: NISPE-1; NISPE-2; SE; SEO; SEOW; SEW; SJE; SJEO; SJEOW; SJEW; SPE-1; SPE-2; SPE-3; SRDE; SVE; SVEO; TF; TFF; THHW; THW; TW Agency Ratings: UL Class 11; UL Class 12; UL Class 36; UL Class 43; UL QMTT2 .E73402 Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.28 g/cc
1.28 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
15 seconds; ASTM D2240
Tensile Strength at Break 17.9 MPa
2600 psi
ASTM D638
Elongation at Break 250 %
250 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Continuous Use; ASTM D794
Brittleness Temperature -45.0 °C
-49.0 °F
ASTM D746
Oxygen Index 26 %
26 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 5.80e+13 ohm-cm
5.80e+13 ohm-cm
ASTM D257
Dielectric Constant 3.34

@Frequency 1.00e+6 Hz
3.34

@Frequency 1.00e+6 Hz
ASTM D150
4.98

@Frequency 1000 Hz
4.98

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.056

@Frequency 1000 Hz
0.056

@Frequency 1000 Hz
ASTM D150
0.088

@Frequency 1.00e+6 Hz
0.088

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Appearance Opaque