Teknor Apex APEX® 121 Polyvinyl Chloride, Flexible

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Wire and Cable Grade
Manufacturer Teknor Apex Company
Trade Name APEX®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Teknor Apex APEX® 121 Polyvinyl Chloride, Flexible.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Notes: 90°C Jacket; RoHS Compliant Features: Good UV Resistance Uses: Telephone Drop Wire Insulation; Telephone Drop Wire JacketingAgency Ratings: REA Unspecified Rating Forms: PelletsInformation Provided by Teknor Apex
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore C 83
83
10 seconds; ASTM D2240
Tensile Strength at Break 17.2 MPa
2500 psi
ASTM D638
Elongation at Break 360 %
360 %
ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 90.0 °C
194 °F
Continuous Use; ASTM D794
Brittleness Temperature -51.0 °C
-59.8 °F
ASTM D746
Oxygen Index 27 %
27 %
ASTM D2863
Descriptive Properties Value Comments
Appearance Opaque