Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength at Break | 17.2 MPa | 2500 psi | TM R050-36 |
Resinlab® EP1285HD-12 Highly Filled, Medium Viscosity Casting Resin Resinlab™ EP1285 (Formerly Lab Product W021901 series) is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity and a low C.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | 2 in/min; ASTM D638 |
RheTech Products FT1055-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | 2 in/min; ASTM D638 |
RheTech Products FT1055-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversInterior trimSplash shieldsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | 2 in/min; ASTM D638 |
RheTech Products FT7016-01 Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | 2 in/min; ASTM D638 |
RheTech Products FT7016-01UV Thermoplastic Polyolefin, UV Stabilized, Black Applications: Bumper coversCladdingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | 2 in/min; ASTM D638 |
RheTech Products HP800-706UV 20% Talc Reinforced High Performance Polypropylene Copolymer, Scratch Resistant, UV Stabilized, Impact Modified, SWB White Applications: Interior trim/Instrument panel componentsA/B pillarsGlove box doorsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | chs 20 in; ASTM D412 |
Network Polymers Softflex® 1104 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D4745 |
3M Dyneon™ CC105 Custom Fluoropolymer Compound
(discontinued **) This compound consists of a mixture of 25% fiberglass blended with PTFEInformation provided by Dyneon, A 3M Company |
|||
Tensile Strength at Break | 17.2 - 20.7 MPa | 2500 - 3000 psi | |
ITW Plexus Plexusâ„¢ MA556 Methacrylate Adhesive Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.Standard for structural bonding in the marine industry.Information provided by Illinois Tool Works.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
Teknor Apex APEX® 1020 Polyvinyl Chloride, Semi-Rigid Notes: 60°C General Purpose; RoHS Compliant Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molde.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
Teknor Apex APEX® 121 Polyvinyl Chloride, Flexible Notes: 90°C Jacket; RoHS Compliant Features: Good UV Resistance Uses: Telephone Drop Wire Insulation; Telephone Drop Wire JacketingAgency Ratings: REA Unspecified Rating Forms: PelletsInformation.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
Teknor Apex APEX® 585 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Features: General Purpose Uses: Tubing; Wire Jacketing Agency Ratings: UL 498; UL 62 Wire Types: SPT-1; SPT-2 Processing Method: ExtrusionForms: PelletsInformation Provided by .. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
Teknor Apex APEX® 65014 Polyvinyl Chloride, Flexible Notes: 75°C Jacket; RoHS Compliant Uses: Wire and Cable ApplicationsForms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
Teknor Apex APEX® 77-W115-B Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Uses: Connects; Grommets; Plugs; Strain ReliefsForms: Pellets Agency Ratings: UL QMFZ2 .E54709 Wire Types: Molded Components Additional Information: T.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D412 |
Teknor Apex Monprene® MP-1287A Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
Teknor Apex APEX® 830 Polyvinyl Chloride, Flexible Notes: 105°C Jacket; RoHS Compliant Features: Low Temperature Flexibility; High Heat Resistance; Oil Resistance Uses: Cable Jacketing Forms: Pellets Wire Types: SJT; ST; SVT; SRDT Processing Meth.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D412 |
Teknor Apex Telcar® TL-1472A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
ExxonMobil LLDPE LL 1002YB Wire & Cable Linear Low Density Polyethylene Resin Product Description: LL 1002YB is a C4 Ziegler Natta LLDPE for Low Voltage power cable and Telecom jacketing. The grade contains a higher level of antioxidants and has excellent Environmental Stress.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | 20 in/min; ASTM D638 |
ExxonMobil PP9074MED Polypropylene Homopolymer Product Description: A highly clarified random copolymer resin designed for injection molding of medical devices suitable for sterilization by high energy radiation.Availability: Europe and North A.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
Teknor Apex APEX® 7500-85 Polyvinyl Chloride, Flexible Notes: 105°C General Purpose; RoHS Compliant Features: High Heat Resistance Uses: Connectors; Grommets; Plugs; Strain ReliefsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL Q.. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
Teknor Apex APEX® 97-G0029B-80 Polyvinyl Chloride, Flexible Notes: RoHS Compliant Uses: Wire and Cable Applications Forms: PelletsInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D412 |
Teknor Apex Monprene® MP 1566 Thermoplastic Elastomer Notes: Translucent Features: Super Tough; Excellent Melt Strength; Good Chemical and Oil ResistanceInformation Provided by Teknor Apex |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 402 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 402 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Tensile Strength at Break | 17.2 MPa | 2500 psi | ASTM D638 |
A. Schulman POLYTROPE™ TPP 508 Injection Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 508 is an injection molding grade olefinic thermoplastic elastomer. This product has excellent low temperature impact properties and flow characteristics suitable for moldi.. |