Techmer ES HiFill® HDPE GF30 A1 30% Glass Filled

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Glass fiber Filled
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® HDPE GF30 A1 30% Glass Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 30% Filler by WeightInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Water Absorption 0.030 %

@Time 86400 sec
0.030 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm

@Thickness 3.17 mm
0.0030 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 76
76
ASTM D785
Tensile Strength, Yield 55.8 MPa
8100 psi
ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Flexural Strength 68.9 MPa
10000 psi
ASTM D790
Flexural Modulus 3.79 GPa
550 ksi
ASTM D790
Izod Impact, Notched 1.12 J/cm

@Thickness 3.17 mm
2.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.87 J/cm

@Thickness 3.17 mm
11.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 54.0 µm/m-°C
30.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 129 °C
265 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
Unannealed; ASTM D648
Flammability, UL94 HB
HB