Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1013STHL Nylon 6/6 (DAM) Information provided by Ravago. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
PolyOne Geon™ 80510 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Ravago Manufacturing Americas Hylon® N1013STL Nylon 6/6 (DAM)
(discontinued **) Information provided by Ravago. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | Tangent; ASTM D790 |
Fiberfil® J-60/20 Polypropylene Homopolymer, 20% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | Tangent; ASTM D790 |
Fiberfil® J-60/20/E/HF Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1510A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1510 compound is a 10% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Techmer ES Elastoblend® PA6/6 GF13 IM2 BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU), Glass Fiber Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical res.. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Techmer ES HiFill® PA6/6 GF5 HS L 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Lubricant and Heat StabilizerFeatures: Lubricated and Heat StabilizedAppearance.. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Techmer ES Plaslube® J-50/10/TF/10 Polycarbonate, 10% GFR, 10% PTFE |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Teknor Apex Chemlon® 104-13 GH Nylon 66, 13% Glass Fiber Reinforced Notes: Impact Modified; Reinforced with 13% Glass Fibers; Synergistic compound exhibiting impact strength and dimensional stability Features: Good Dimensional stability; Good Processability; Heat St.. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
A. Schulman ComAlloy® 510-3010 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | Initial flexural modulus |
Fibre Glast 88 / 87 General Purpose Epoxy Resin and Hardener
(discontinued **) Description:#88 Epoxy Resin is a 100% reactive low viscosity liquid bisphenol-A based epoxy resin diluted with Alkyl glycidyl ether. This resin is specially designed for applications requiring low v.. |
|||
Flexural Modulus | 3.79 GPa | 550 ksi | ASTM D790 |
Techmer ES HiFill® PA4/6 GF5 HS 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedInformation provided by TP Composites, .. |