Techmer ES Electrablend® POM CO Acetal

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, Unreinforced
Manufacturer Techmer ES
Trade Name Electrablend®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES Electrablend® POM CO Acetal.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFeatures: Copolymer and Medium ViscosityInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.41 g/cc
0.0509 lb/in³
ASTM D792
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.018 cm/cm

@Thickness 3.17 mm
0.018 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D785
Tensile Strength, Yield 62.1 MPa
9000 psi
ASTM D638
Elongation at Break 30 %
30 %
ASTM D638
Flexural Strength 81.4 MPa
11800 psi
ASTM D790
Flexural Modulus 2.83 GPa
410 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm

@Thickness 3.17 mm
1.10 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 21.6 µm/m-°C
12.0 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 160 °C
320 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 110 °C
230 °F
Unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 1000 - 1.00e+6 ohm-cm
1000 - 1.00e+6 ohm-cm
ASTM D257
Surface Resistance 1000 - 1.00e+6 ohm
1000 - 1.00e+6 ohm
ASTM D257
Shielding Effectiveness 40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
40 dB

@Frequency 3.00e+7 - 1.00e+9 Hz
ASTM D149