Polymer Property : 300% Modulus = 0.0147 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
300% Modulus 0.0147 GPa
2.13 ksi
150°C, 40 min., Pressure Vulcanization. 38% Change after 100°C, 70 hrs, Oil Immersion
KKPC KOSYN KNB 0230L Acrylonitrile Butadiene Rubber (NBR)
Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. ..
300% Modulus 0.0147 GPa
2.13 ksi
150°C, 40 min., Pressure Vulcanization. 40% Change after 100°C, 70 hrs, Oil Immersion
KKPC KOSYN KNB 35M Acrylonitrile Butadiene Rubber (NBR)
Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. ..
300% Modulus 0.0147 GPa
2.13 ksi
150°C, 40 min., Pressure Vulcanization. 45% Change after 100°C, 70 hrs, Oil Immersion
KKPC KOSYN KNB 40M Acrylonitrile Butadiene Rubber (NBR)
Acrylonitrile Butadiene Rubber (NBR)Characteristics: KOSYN KNB is copolymer of high oil resistance and chemical resistance made from acrylonitrile and butadiene by the cold emulsion polymerization. ..
300% Modulus 0.0147 GPa
2.13 ksi
Taiwan PU Corporation TPUI-G90 High Wear Resistance, Injection Molding Polycaprolactone Base TPU
Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation.
300% Modulus 0.0147 GPa
2.13 ksi
Taiwan PU Corporation TPUI-L90 Low Temperature Resistance, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
300% Modulus 0.0147 GPa
2.13 ksi
Taiwan Sheen Soon Sheenthane® A8670A Film Grade Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for blown filmWaterproof & breathable gradeInformation provided by Taiwan Sheen Soon Co., LTD.
300% Modulus 0.0147 GPa
2.13 ksi
Taiwan Sheen Soon Sheenthane® A8700F Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
300% Modulus 0.0147 GPa
2.13 ksi
Taiwan Sheen Soon Sheenthane® A8900F Thermoplastic Polyurethane Elastomer
Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD.
300% Modulus 0.0147 GPa
2.13 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
300% Modulus 0.0147 GPa
2.13 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 2.0 PHR MBT
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..