Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Taiwan PU Corporation TPU-CH85 High Hydrolysis Resistance, Calender Molding Polyether Base TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer Taiwan PU Corporation
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Taiwan PU Corporation TPU-CH85 High Hydrolysis Resistance, Calender Molding Polyether Base TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Calender MoldingInformation provided by Taiwan PU Corporation.
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Tensile Strength at Break 21.57 MPa
3128 psi
Elongation at Break 950 %
950 %
100% Modulus 0.00590 GPa
0.856 ksi
300% Modulus 0.00590 GPa
0.856 ksi
Resilience 60
60
%, Impact Resilience
Taber Abrasion, mg/1000 Cycles 26
26
Processing Properties Metric English Comments
Feed Temperature 170 °C
338 °F
Middle Barrel Temperature 175 °C
347 °F
Compress zone
Front Barrel Temperature 180 °C
356 °F
Metering zone
Adapter Temperature 185 °C
365 °F
Die Temperature 185 °C
365 °F