Polymer Property : Middle Barrel Temperature = 175 °C Product List

Processing Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Processing Properties Metric English Comments
Middle Barrel Temperature 175 - 195 °C
347 - 383 °F
Huntsman AVALON® 80 ABX Thermoplastic Polyurethane
Introduction: AVALON 80 ABX is a high performance polyester based thermoplastic polyurethane for injection molding. AVALON 80 ABX is part of the AVALON Perform Range and offers a specially designed,..
Middle Barrel Temperature 175 °C
347 °F
Extrusion
Huntsman IROGRAN® A 94 E 4900 TPU-Polyester
Introduction: IROGRAN A 94 E 4900 is a thermoplastic polyester polyurethane for melt calendering. IROGRAN is part of the HUNTSMAN technical extrusion/injection molding product range and offers a spe..
Middle Barrel Temperature 175 - 215 °C
347 - 419 °F
Blow Molding
LG Chemical HYPERIER IP1306B PA-HDPE Nanoclay Compound
HYPERIER is a nano compound made from nano-sized inorganic plate clay. Blow Molding, Barrier thermoplastic, Nylon blend with HDPEApplication: Agrochemical Container, SORE* Fuel Tank, PFCCAS No. 900..
Middle Barrel Temperature 175 - 195 °C
347 - 383 °F
KEP Kepital® F20 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 175 - 195 °C
347 - 383 °F
KEP Kepital® F20-52 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 175 - 195 °C
347 - 383 °F
KEP Kepital® F30 Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 175 - 195 °C
347 - 383 °F
KEP Kepital® FG2025 25% Glass Fiber Reinforced Acetal Copolymer
Information provided by US distributor Polymer Technology and Services, LLC (PTS).
Middle Barrel Temperature 175 - 190 °C
347 - 374 °F
Huntsman AVALON® 70 AE Thermoplastic Polyurethane
Introduction: AVALON 70 AE is a general purpose polyester based thermoplastic polyurethane for injection molding. AVALON 70 AE is part of the AVALON Soft Range and offers a premium soiling material ..
Middle Barrel Temperature 175 - 185 °C
347 - 365 °F
Extrusion
Huntsman IROGRAN® A 87 P 4946 TPU-Polyester
Introduction: IROGRAN A 87 P 4946 is a polyether based thermoplastic polyurethane intended for injection molding and extrusion applications. IROGRAN A 87 P 4946 is part of the HUNTSMAN technical ext..
Middle Barrel Temperature 175 °C
347 °F
Compress zone
Taiwan PU Corporation TPU-C85 General Grade, Calender Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Calender MoldingInformation provided by Taiwan PU Corporation.
Middle Barrel Temperature 175 °C
347 °F
Compress zone
Taiwan PU Corporation TPU-CH85 High Hydrolysis Resistance, Calender Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Calender MoldingInformation provided by Taiwan PU Corporation.
Middle Barrel Temperature 175 °C
347 °F
Compress zone
Taiwan PU Corporation TPU-EH80 High Hydrolysis Resistance, Extrusion Molding Polyether Base TPU
Thermoplastic Polyurethane (TPU), High Hydrolysis Resistance, Polyether Base, Extrusion MoldingInformation provided by Taiwan PU Corporation.
Middle Barrel Temperature 175 °C
347 °F
Compress zone
Taiwan PU Corporation TPUI-E80 General Grade, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Middle Barrel Temperature 175 °C
347 °F
Compress zone
Taiwan PU Corporation TPUI-L75 Low Temperature Resistance, Injection Molding Polyester Base TPU
Thermoplastic Polyurethane (TPU), Low Temperature Resistance, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation.
Middle Barrel Temperature 175 °C
347 °F
Blow Film
DuPont Nucrel® 30907 Ethylene Acid Copolymer Resin
Nucrel® 30907 is an ethylene acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminating equipment designed to process polyethylene resin..
Middle Barrel Temperature 175 - 245 °C
347 - 473 °F
Equate EMDA-8920 HDPE Injection Molding Resin
EMDA-8920 is a high density copolymer polyethylene resin designed for injection molding applications which require excellent toughness and gloss.Applications: EMDA-8920 is a high density copolymer p..