TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 93A

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 93A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear strength, oil and fuel resistance, and ozone resistance. The life expectancy of urethane is often 5 times longer than other elastomers, thus saving material costs and downtime expense. One shortcoming of polyurethanes is loss of physical properties at temperatures over 180°F (82°C). MILLATHANE HT has overcome this weakness.Non-Black with Peroxide Cure SystemFormulationMillathane HT100.0Hi-Sil 243 LD60.0Di-Cup 40C1.0All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 93
93
Tensile Strength, Yield 19.73 MPa
2861 psi
Elongation at Yield 343 %
343 %
100% Modulus 0.007288 GPa
1.057 ksi
200% Modulus 0.01298 GPa
1.882 ksi
300% Modulus 0.01708 GPa
2.477 ksi
Tear Strength 62.1 kN/m
354 pli
Die C
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 160 °C
0.167 hour

@Temperature 320 °F