Mechanical Properties | Metric | English | Comments |
---|---|---|---|
200% Modulus | 0.01298 GPa | 1.882 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 93A MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
200% Modulus | 0.01298 GPa | 1.882 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 93A MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |