Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.01708 GPa | 2.477 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 93A MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
300% Modulus | 0.01708 GPa | 2.477 ksi | |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, Hardness 93A MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |