Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 46A

Category Polymer , Thermoset , Polyester, TS , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced , Rubber or Thermoset Elastomer (TSE)
Manufacturer TSE Industries, Inc
Trade Name Millathane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 46A.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed for applications in shoe soling, roll coverings and all other applications where transparent, brightly colored or decorative products are desired.FormulationMillathane 97 100Stearic Acid0.2Wacker HDK-N2015Mediaplast NB-415Silquest A-1720.3Irganox 10100.25Tinuvin 3280.25Tinuvin 7650.25Luperox 2310.5All information provided by TSE Industries
Mechanical Properties Metric English Comments
Hardness, Shore A 46
46
Tensile Strength, Yield 7.398 MPa
1073 psi
Elongation at Yield 530 %
530 %
100% Modulus 0.000972 GPa
0.141 ksi
200% Modulus 0.00130 GPa
0.189 ksi
300% Modulus 0.00170 GPa
0.247 ksi
Tear Strength 12.1 kN/m
69.0 pli
Die C
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
transparent; thickness not quantified
Processing Properties Metric English Comments
Cure Time 10.0 min

@Temperature 149 °C
0.167 hour

@Temperature 300 °F
Users viewing this material also viewed the following: