Mechanical Properties Metric English Comments
200% Modulus 0.00130 GPa
0.189 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 46A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..
200% Modulus 0.00130 GPa
0.189 ksi
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 46A
Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed ..