Mechanical Properties | Metric | English | Comments |
---|---|---|---|
300% Modulus | 0.00170 GPa | 0.247 ksi | ISO/R527 |
Polykemi AB POLYelast TPE Z300 Thermoplastic Elastomer, SEBS-based Information provided by Polykemi AB |
|||
300% Modulus | 0.00170 GPa | 0.247 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 46A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |
|||
300% Modulus | 0.00170 GPa | 0.247 ksi | |
TSE Industries Millathane® 97 Millable Polyester Polyurethane Rubber, Hardness 46A Millathane 97 is a polyether polyurethane rubber having excellent transparency, good wear properties, a high coefficient of friction and very good UV stability. This polyurethane rubber is designed .. |