Stellar Canada CERAMITE® CSR-S Wear Resistant Castable

Category Ceramic , Carbide , Oxide
Manufacturer Stellar Canada
Trade Name CERAMITE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Stellar Canada CERAMITE® CSR-S Wear Resistant Castable.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world wide, both as mortars and as various precast components. Ceramite can easily be mixed, cast and shaped in any size and is thus comfortably to work with in-situ. Ceramite can be used in within a wide range of temperatures and applications exposed to thermal shock conditions in industries like for example aluminum, cement and ferro.Applications: Floor Tile, Hearth/Furnace Tile, Furnace Sills & Doors, Lintels, Pipe and Duct Linings, Feed Tubes, Troughs/Launders, Ladles, Dampers, Nozzle Blasters, Crucible Linings, Vortex, Burner Tip Cooler Plates, Nose Ring, Electrical Insulation, Cold Wear AreasSpecific Notes on This Grade: A castable with extreme abrasion resistance and high thermal conductivity. Used in the same industries as BKR in areas with high abrasion problems. References as lining material for pipes and bends, impact plates, lining of transportation systems, duct linings, crucible linings etc...Information provided by Stellar Canada.
Physical Properties Metric English Comments
Bulk Density 2.79 g/cc
0.101 lb/in³
Self-flowing
Mechanical Properties Metric English Comments
Modulus of Rupture 0.02800 GPa
4.061 ksi
Hot, prefired at 1832°F/24 hours (1000°C)
Flexural Strength 18.33 MPa

@Temperature 850.0 °C
2659 psi

@Temperature 1562 °F
after Firing; ASTM-349
20.40 MPa

@Temperature 500 °C
2959 psi

@Temperature 932 °F
after Firing; ASTM-349
21.40 MPa

@Temperature 1000 °C
3104 psi

@Temperature 1832 °F
after Firing; ASTM-349
23.17 MPa

@Temperature 1200 °C
3361 psi

@Temperature 2192 °F
after Firing; ASTM-349
Compressive Strength 115.0 MPa

@Temperature 1200 °C
16680 psi

@Temperature 2190 °F
after Firing; ASTM C-349
119.0 MPa

@Temperature 1000 °C
17260 psi

@Temperature 1830 °F
after Firing; ASTM C-349
133.0 MPa

@Temperature 850 °C
19290 psi

@Temperature 1560 °F
after Firing; ASTM C-349
137.0 MPa

@Temperature 20.0 °C
19870 psi

@Temperature 68.0 °F
after 7 days
176.00 MPa

@Temperature 500 °C
25527 psi

@Temperature 932 °F
after Firing; ASTM C-349
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1000 °C
1832 °F
Component Elements Properties Metric English Comments
Al2O3 21 %
21 %
CaO 4.3 %
4.3 %
Fe2O3 0.030 %
0.030 %
K2O 0.020 %
0.020 %
MgO 0.010 %
0.010 %
Na2O 0.050 %
0.050 %
SiC 64 %
64 %
SiO2 10 %
10 %
Descriptive Properties Value Comments
Application Prefired
Precast Shapes