Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Compressive Strength | 137.0 MPa @Temperature 20.0 °C |
19870 psi @Temperature 68.0 °F |
after 7 days |
Stellar Canada CERAMITE® CSR-S Wear Resistant Castable Ceramite is a family of wear resistant castables with a unique combination of high wear resistance, thermal resistance and mechanical strength. Ceramite is produced and supplied to end users world w.. |