Eagle Brass 301 Austenitic Stainless Steel, Annealed

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer Eagle Brass Company
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Eagle Brass 301 Austenitic Stainless Steel, Annealed.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Type 301 is a chromium-nickel stainless steel that provides high strength and good ductility with chromium and nickel contents lowered to increase the work hardening range. This permits higher tensile strengths to be achieved by rolling with a lower loss of ductility. When this grade is cold worked it becomes more magnetic than other austenitic stainless steels. Typical uses include aircraft structural parts, diaphragms, utensils, automotive trim, and conveyor belts.Information provided by Eagle Brass Company
Physical Properties Metric English Comments
Density 7.89 g/cc
0.285 lb/in³
As Annealed
Mechanical Properties Metric English Comments
Tensile Strength >= 517 MPa
>= 75000 psi
Tensile Strength, Yield >= 207 MPa
>= 30000 psi
0.2% Offset
Elongation at Break >= 40 %
>= 40 %
in 2 inches
Tensile Modulus 193 GPa
28000 ksi
Thermal Properties Metric English Comments
CTE, linear 18.7 µm/m-°C

@Temperature 20.0 - 649 °C
10.4 µin/in-°F

@Temperature 68.0 - 1200 °F
Thermal Conductivity 16.3 W/m-K
113 BTU-in/hr-ft²-°F
Component Elements Properties Metric English Comments
Carbon, C <= 0.15 %
<= 0.15 %
Chromium, Cr 16 - 18 %
16 - 18 %
Iron, Fe 74.775 - 78 %
74.775 - 78 %
Calculated as Balance
Manganese, Mn <= 2.0 %
<= 2.0 %
Nickel, Ni 6.0 - 8.0 %
6.0 - 8.0 %
Phosphorous, P <= 0.045 %
<= 0.045 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %