Material Notes:
Boron & Graphite prepreg. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 mil boron fibers, Hy-Bor material can be manufactured to incorporate any commercially available graphite prepreg. By altering the spacing of the boron fiber in the prepreg, performance properties and material costs can be tailored to meet the needs of a variety of demanding applications. Information provided by Specialty Materials, Inc.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1896 MPa
275000 psi
Elongation at Yield 0.80 %
0.80 %
Modulus of Elasticity 241 GPa
35000 ksi
Flexural Yield Strength 2413 MPa
350000 psi
Flexural Modulus 214 GPa
31000 ksi
Compressive Yield Strength 2756 MPa
399700 psi
Compressive Modulus 241 GPa
35000 ksi
Shear Strength 103 MPa
14900 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 177 °C
351 °F
Processing Properties Metric English Comments
Processing Temperature 121 °C
250 °F