Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Modulus of Elasticity = 35000 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 241 GPa
35000 ksi
Specialty Materials Hy-Bor Boron/Graphite Hybrid Prepreg Tape
Boron & Graphite prepreg. Combining Specialty Materials' boron fiber with graphite prepreg, Hy-Bor® is a high-performance material with exceptional properties. Available with 4.0 and 5.6 mil..
Modulus of Elasticity 241 GPa
35000 ksi
Tensile modulus calculated at secant 6000-1000
Hexcel® AS4D Carbon Fiber (12,000 Filaments)
Weight/length = 0.765 g/m.Information provided by Hexcel Corporation. Values are typical average lot properties.Continuous fiber can be combined with virtually all thermoset and thermoplastic resin..
Modulus of Elasticity 241 GPa
35000 ksi
In Tension
Cytec Thornel® T-650/35 3K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Modulus of Elasticity 241 GPa
35000 ksi
In Tension
Cytec Thornel® T-650/35 6K Carbon Fiber, Polyacrylonitrile (PAN) Precursor
Data provided by the manufacturer, Amoco Performance Products, Inc.Continuous length, high strength, high modulus fiber made from a polyacrylonitrile precursor. The fiber surface has been treated t..
Modulus of Elasticity 241 GPa
35000 ksi
CMW® THERMKON® 70M Molybdenum Copper parts
For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc.
Modulus of Elasticity 241 GPa
35000 ksi
CMW® THERMKON® 76 Tungsten Copper parts
For matching CTE of semiconductor substrates while allowing high thermal transfer.Information provided by CMW Inc.
Modulus of Elasticity 241 GPa
35000 ksi
At 45° to rolling direction
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 241 GPa
35000 ksi
At 45° to rolling direction
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 241 GPa
35000 ksi
At 45° to rolling direction
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 241 GPa
35000 ksi
At 45° to rolling direction
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 241 GPa
35000 ksi
At 45° to rolling direction
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Modulus of Elasticity 241 GPa
35000 ksi
At 45° to rolling direction
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Copyright © lookpolymers.com All Rights Reserved