Specialty Coating Systems Parylene C Poly (P-Xylylene) Coating

Category Polymer , Film , Thermoplastic , Poly (P-Xylylene)
Manufacturer Specialty Coating Systems (SCS)
Trade Name Parylene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Specialty Coating Systems Parylene C Poly (P-Xylylene) Coating.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Parylene C is a polymer of para-xylylene modified by the substitution of a chlorine atom for one of the aromatic hydrogen atoms. Parylene C has a useful combination of electrical and physical properties, plus a very low permeability to moisture and corrosive gases.SCS Parylene conformal coatings are ultra-thin, pinhole-free polymer coatings that provide a number of high-value surface treatment properties such as excellent moisture, chemical and dielectric barrier properties, thermal and UV stability, and dry-film lubricity. Parylene coatings are used in a number of applications throughout the medical device, electronics, automotive, military and aerospace industries.Information provided by Specialty Coating Systems (SCS) .
Physical Properties Metric English Comments
Water Vapor Permeability 0.0800 g mil/ (m2 day)

@Temperature 37.0 °C
0.00516 g mil/ (100 in2 day)

@Temperature 98.6 °F
90% RH; ASTM F1249
Density 1.289 g/cc
0.04657 lb/in³
ASTM D1505
Water Absorption <= 0.10 %

@Time 86400 sec
<= 0.10 %

@Time 24.0 hour
ASTM D570
Oxygen Transmission 2.80 cc-mm/m²-24hr-atm

@Temperature 25.0 °C
7.11 cc-mil/100 in²-24hr-atm

@Temperature 77.0 °F
ASTM D1434
Nitrogen Transmission 0.400 cc-mm/m²-24hr-atm

@Temperature 25.0 °C
1.02 cc-mil/100 in²-24hr-atm

@Temperature 77.0 °F
ASTM D1434
Carbon Dioxide Transmission 3.00 cc-mm/m²-24hr-atm

@Temperature 25.0 °C
7.62 cc-mil/100 in²-24hr-atm

@Temperature 77.0 °F
ASTM D1434
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength 68.9 MPa
10000 psi
Tensile Strength, Yield 55.2 MPa
8000 psi
ASTM D882
Elongation at Break <= 200 %
<= 200 %
ASTM D882
Elongation at Yield 2.9 %
2.9 %
ASTM D882
Modulus of Elasticity 2.76 GPa
400 ksi
Secant; ASTM D882
Coefficient of Friction, Dynamic 0.29
0.29
ASTM D1894
Coefficient of Friction, Static 0.29
0.29
ASTM D1894
Thermal Properties Metric English Comments
CTE, linear 35.0 µm/m-°C
19.4 µin/in-°F
via TMA
Specific Heat Capacity 0.712 J/g-°C
0.170 BTU/lb-°F
Thermal Conductivity 0.0840 W/m-K
0.583 BTU-in/hr-ft²-°F
ASTM C177
Melting Point 290 °C
554 °F
via DSC
Maximum Service Temperature, Air 80.0 °C
176 °F
Continuous
100 °C
212 °F
Short Term
Softening Point 125 °C
257 °F
T5 Point; modulus = 690 MPa (100,000 psi)
240 °C
464 °F
T4 point; modulus = 70 MPa (10,000 psi)
Optical Properties Metric English Comments
Refractive Index 1.639
1.639
n<sub>D</sub>; Abbe Refractometer
Transmission, Visible 86 %

@Wavelength 400 nm
86 %

@Wavelength 400 nm
UV Transmittance <= 1.0 %

@Wavelength 281 nm
<= 1.0 %

@Wavelength 281 nm
cutoff
75 %

@Wavelength 300 nm
75 %

@Wavelength 300 nm
82 %

@Wavelength 350 nm
82 %

@Wavelength 350 nm
Electrical Properties Metric English Comments
Volume Resistivity 8.80e+16 ohm-cm
8.80e+16 ohm-cm
50% RH; ASTM D257
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
50% RH; ASTM D257
Dielectric Constant 2.95

@Frequency 1.00e+6 Hz
2.95

@Frequency 1.00e+6 Hz
ASTM D150
3.1

@Frequency 1000 Hz
3.1

@Frequency 1000 Hz
ASTM D150
3.15

@Frequency 60.0 Hz
3.15

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 220 kV/mm
5600 kV/in
ASTM D149
Dissipation Factor 0.013

@Frequency 1.00e+6 Hz
0.013

@Frequency 1.00e+6 Hz
ASTM D150
0.019

@Frequency 1000 Hz
0.019

@Frequency 1000 Hz
ASTM D150
0.020

@Frequency 60.0 Hz
0.020

@Frequency 60.0 Hz
ASTM D150
Compliance Properties Metric English Comments
USP Class VI Yes
Yes
Descriptive Properties Value Comments
Biocompatibility ISO 10993
Hydrogen Transmission 43.3 cc-mm/m²-24hr-atm
ASTM D1434
UV Stability > 2000 hours
ASTM G154