Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.711 J/g-°C | 0.170 BTU/lb-°F | |
GrafTech eGRAF® HITHERM™ HT-2505 Graphite with Polymer Additive Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Specific Heat Capacity | 0.711 J/g-°C | 0.170 BTU/lb-°F | |
GrafTech eGRAF® HITHERM™ HT-2510 Graphite with Polymer Additive Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Specific Heat Capacity | 0.711 J/g-°C | 0.170 BTU/lb-°F | |
GrafTech eGRAF® HITHERM™ HT-705 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Specific Heat Capacity | 0.711 J/g-°C | 0.170 BTU/lb-°F | |
GrafTech eGRAF® HITHERM™ HT-710 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Specific Heat Capacity | 0.711 J/g-°C | 0.170 BTU/lb-°F | |
GrafTech eGRAF® HITHERM™ HT-720 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Specific Heat Capacity | 0.712 J/g-°C | 0.170 BTU/lb-°F | |
Mateck Silicon (Si) Optical crystals |
|||
Specific Heat Capacity | 0.711 J/g-°C | 0.170 BTU/lb-°F | |
GrafTech eGRAF® HITHERM™ HT-1205 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Specific Heat Capacity | 0.711 J/g-°C | 0.170 BTU/lb-°F | |
GrafTech eGRAF® HITHERM™ HT-1210 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Specific Heat Capacity | 0.711 J/g-°C | 0.170 BTU/lb-°F | |
GrafTech eGRAF® HITHERM™ HT-1220 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Specific Heat Capacity | 0.710 J/g-°C | 0.170 BTU/lb-°F | |
Schott N-SF11 Glass Information Provided by SCHOTT North America, Inc. |
|||
Specific Heat Capacity | 0.710 J/g-°C | 0.170 BTU/lb-°F | |
Specialty Materials SCS-6 Silicon Carbide Monofilament High strength at high temperature. These fibers are used in metal, ceramic and polymer matrix composites and are extremely effective for high-temperature applications. Silicon carbide reinforced tit.. |
|||
Specific Heat Capacity | 0.712 J/g-°C | 0.170 BTU/lb-°F | |
Specialty Coating Systems Parylene C Poly (P-Xylylene) Coating Parylene C is a polymer of para-xylylene modified by the substitution of a chlorine atom for one of the aromatic hydrogen atoms. Parylene C has a useful combination of electrical and physical proper.. |
|||
Specific Heat Capacity | 0.710 J/g-°C | 0.170 BTU/lb-°F | |
Cytec Thornel® VCB-20 Carbon Fiber Cloth Data provided by the manufacturer, Amoco Performance Products, Inc.Used as a reinforcement in structural, ablative, and abrasion-resistant composites.2000 filaments/strand, 99+% carbon assayThornel®.. |