Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Special Metals INCONEL® MA758 Oxide-Dispersion-Strengthened Ni-Cr Superalloy

Category Metal , Nonferrous Metal , Nickel Alloy , Superalloy
Manufacturer Special Metals (includes the former Inco Alloys International Inc.)
Trade Name INCONEL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Special Metals INCONEL® MA758 Oxide-Dispersion-Strengthened Ni-Cr Superalloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Special Metals.
Physical Properties Metric English Comments
Density 8.14 g/cc
0.294 lb/in³
Thermal Properties Metric English Comments
CTE, linear 12.47 µm/m-°C

@Temperature 25.0 - 92.0 °C
6.928 µin/in-°F

@Temperature 77.0 - 198 °F
Mean
13.18 µm/m-°C

@Temperature 25.0 - 316 °C
7.322 µin/in-°F

@Temperature 77.0 - 601 °F
Mean
14.11 µm/m-°C

@Temperature 25.0 - 482 °C
7.839 µin/in-°F

@Temperature 77.0 - 900 °F
Mean
15.03 µm/m-°C

@Temperature 25.0 - 760 °C
8.350 µin/in-°F

@Temperature 77.0 - 1400 °F
Mean
Melting Point >= 1375 °C
>= 2507 °F
Solidus 1375 °C
2507 °F
Maximum Service Temperature, Air 1260 °C
2300 °F
for demanding high temp uses
Component Elements Properties Metric English Comments
Aluminum, Al <= 0.30 %
<= 0.30 %
Carbon, C 0.050 %
0.050 %
Chromium, Cr 30 %
30 %
Iron, Fe 1.0 %
1.0 %
Nickel, Ni 67.5 %
67.5 %
As remainder
Titanium, Ti 0.50 %
0.50 %
Y2O3 0.60 %
0.60 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0001139 ohm-cm
0.0001139 ohm-cm
Users viewing this material also viewed the following: