Electrical Properties Metric English Comments
Electrical Resistivity 0.0001139 ohm-cm
0.0001139 ohm-cm
Special Metals INCONEL® MA758 Oxide-Dispersion-Strengthened Ni-Cr Superalloy
Data provided by the manufacturer, Special Metals.