Polymer Property : Electrical Resistivity = 0.0001139 ohm-cm
Polymer Property :
Electrical Resistivity =
0.0001139 ohm-cm
Product List
Electrical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Electrical Properties
Metric
English
Comments
Electrical Resistivity
0.0001139
ohm-cm
0.0001139
ohm-cm
Special Metals INCONEL® MA758 Oxide-Dispersion-Strengthened Ni-Cr Superalloy
Data provided by the manufacturer, Special Metals.
HOME