Polymer Property : Melting Point = 2507 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Melting Point 1375 °C
2507 °F
Special Metals INCONEL® alloy MA758 Ni-Cr Superalloy
INCONEL® alloy MA 758 is an oxide-dispersion-strengthened (ODS) nickel-chromium superalloy, made by mechanical alloying. It is a development of the well-established aerospace superalloy, INCONEL..
Melting Point >= 1375 °C
>= 2507 °F
Special Metals INCONEL® MA758 Oxide-Dispersion-Strengthened Ni-Cr Superalloy
Data provided by the manufacturer, Special Metals.
Melting Point 1375 °C
2507 °F
Alloy Wire International RW 70 Hot Cutting Wire - High Strength
Maintains high strength at elevated temperatures. Used for cutting expanded polystyrene (EPS) foam and for the heat sealing of polypropylene bags.Information provided by Alloywire International.