Spartech Weather-Pro G Weatherable Sheet

Category Polymer , Thermoplastic
Manufacturer Spartech
Trade Name Weather-Pro
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Spartech Weather-Pro G Weatherable Sheet.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Weatherable SheetInformation provided by Spartech.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Rockwell L 85
85
ASTM D785
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM D638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D638
Flexural Yield Strength 51.7 MPa
7500 psi
ASTM D790
Flexural Modulus 0.0731 GPa
10.6 ksi
ASTM D790
Izod Impact, Unnotched 1.92 J/cm
3.60 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature 20.0 °C
50.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 92.2 °C
198 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 82.2 °C
180 °F
ASTM D648
Flammability, UL94 HB
HB
Optical Properties Metric English Comments
Gloss 90 %
90 %
Gardner; ASTM D2523