Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay TECHNYL® A 32G1 PA66, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 32G1 PA66, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Flame retardant Polyamide 66, unreinforced, heat stabilized, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: This flame retardant grade, UL 94 V-2 (0.8 mm), GWIT 900°C (0,8 mm) offers best in class flammability performance combined with excellent impact and strain properties. It is particularly suitable for molding electrical components such as connections, junction blocks, terminal blocks and connectors. This product is also suitable for use in electrical appliances needing to comply with the IEC 60335-1 regulation.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.32 g/cc
0.0477 lb/in³
ISO 1183/A
Mechanical Properties Metric English Comments
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527 Type 1A
Elongation at Yield 15 %
15 %
ISO 527 type 1 A
Tensile Modulus 2.95 GPa
428 ksi
ISO 527 Type 1A
Charpy Impact Unnotched 13.2 J/cm²
62.8 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 0.600 J/cm²
2.86 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 85.0 °C
185 °F
ISO 75/Af
Flammability, UL94 V-2

@Thickness 0.380 mm
V-2

@Thickness 0.0150 in
1210
V-2

@Thickness 0.800 mm
V-2

@Thickness 0.0315 in
1210
V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
1210
Glow Wire Test 850 °C

@Thickness 0.800 mm
1560 °F

@Thickness 0.0315 in
ISO 60695-2-12
850 °C

@Thickness 1.60 mm
1560 °F

@Thickness 0.0630 in
ISO 60695-2-12
850 °C

@Thickness 3.20 mm
1560 °F

@Thickness 0.126 in
ISO 60695-2-12
875 °C

@Thickness 0.800 mm
1610 °F

@Thickness 0.0315 in
ignition temperature; ISO 60695-2-13
900 °C

@Thickness 1.60 mm
1650 °F

@Thickness 0.0630 in
ignition temperature; ISO 60695-2-13
Electrical Properties Metric English Comments
Comparative Tracking Index 400 V
400 V
Solution A; IEC 60112
Processing Properties Metric English Comments
Feed Temperature 270 °C
518 °F
Front Barrel Temperature 270 - 290 °C
518 - 554 °F
Mold Temperature 60.0 - 80.0 °C
140 - 176 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.20 %
<= 0.20 %
Descriptive Properties Value Comments
Compression Zone 260-280°C
Users viewing this material also viewed the following: